SABIC Innovative Plastics LNP Lubricomp ICP36 PA 6/12 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Lubricomp ICP36 PA 6/12 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* ICP36 is a compound based on Nylon 6/12 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 174 MPa
25200 psi
ASTM D 638
Elongation at Break 1.7 %
1.7 %
ASTM D 638
Tensile Modulus 19.92 GPa
2889 ksi
50 mm/min; ASTM D 638
Flexural Strength 275 MPa
39900 psi
ASTM D 790
Flexural Modulus 16.68 GPa
2419 ksi
ASTM D 790
Izod Impact, Notched 0.850 J/cm

@Temperature 23.0 °C
1.59 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 199 °C

@Thickness 3.20 mm
390 °F

@Thickness 0.126 in
unannealed; ASTM D 648