Material Notes:
LNP* Thermocomp* D351 (experimental grade name as EXTC8143) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, Non-Brominated & Non-Chlorinated Flame Retardant.
Physical Properties Metric English Comments
Density 1.425 g/cc
0.05148 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
Melt Flow 25.2 g/10 min

@Load 2.16 kg,
Temperature 300 °C
25.2 g/10 min

@Load 4.76 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 300 °C
20 g/10 min

@Load 4.76 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
Type I, 5 mm/min; ASTM D638
125 MPa
18100 psi
5 mm/min; ISO 527
Elongation at Break 2.4 %
2.4 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 9.04 GPa
1310 ksi
5 mm/min; ASTM D638
9.08 GPa
1320 ksi
1 mm/min; ISO 527
Flexural Strength 179 MPa
26000 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 169 MPa
24500 psi
2 mm/min; ISO 178
Flexural Modulus 7.52 GPa
1090 ksi
2 mm/min; ISO 178
8.39 GPa
1220 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.50 J/cm
2.81 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.08 J/cm
9.52 ft-lb/in
ASTM D4812
Charpy Impact Unnotched 3.90 J/cm²
18.6 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 24.0 J
17.7 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 116 °C

@Thickness 3.20 mm
241 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL 94