Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ DP-8928-2-8001 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 604 35 HS Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
SABIC B4660/B4660AB High Density Polyethylene for Blow Molding Product Description: B4660 series grades are medium molecular weight High Density Polyethylene homopolymer for blow molding applications. They are primarily designed for imparting high rigidity, t.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | Izod Impact, double-gated, 23°C; SABIC Method |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific) Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML6413 PC (Asia Pacific) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® PK2870 PC (Asia Pacific) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® PK2870 PC (Europe-Africa-Middle East) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
SABIC BM6246LS High Density Polyethylene for Blow Molding Product Description: BM6246LS grade is a medium molecular weight High Density Polyethylene homopolymer for blow molding applications. It is primarily designed for imparting high rigidity, toughnes.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
LG Chemical LUCEL HI-515 High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific) LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature 0.000 °C |
2.81 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM Data |
Styron Magnum™ 341 ABS, Low Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
PlastxWorld Veroplas PB3300 Nylon 66 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PD100 Nylon 12, Injection Molding Outstanding polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced 6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 33% Glass Reinforced.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.17 mm |
2.81 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® SEG7 35% Glass Filled PA6 (Dry) Ultramid SEG7 is a 35% glass reinforced, injection molding type 6 nylon requiring high strength, surface aesthetics, and good processability. This product has excellent surface appearance
while mai.. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® R3145-20G PC/PBT Alloy, 20% Glass Reinforced A 20% glass reinforced alloy for high impact, increased mechanical strength, chemical resistance, and thermal properties.Data provided by the manufacturer |