SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Water Absorption 0.28 %

@Time 86400 sec
0.28 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0025 cm/cm

@Time 86400 sec
0.0025 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0035 cm/cm

@Time 86400 sec
0.0035 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength, Yield 72.0 MPa
10400 psi
5 mm/min; ISO 527
Elongation at Break 4.3 %
4.3 %
5 mm/min; ISO 527
Tensile Modulus 3.50 GPa
508 ksi
1 mm/min; ISO 527
Flexural Yield Strength 119 MPa
17300 psi
2 mm/min; ISO 178
Flexural Modulus 3.80 GPa
551 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 47.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
26.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
27.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 176 °C
349 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af