Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | ASTM D955 |
PolyOne LubriOne™ PC-20GF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0050 cm/cm | 0.0025 - 0.0050 in/in | |
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. Glass fibers. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0065 cm/cm | 0.0025 - 0.0065 in/in | |
LATI Latigea B01 I8 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Thickness 3.17 mm |
0.0025 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Thickness 3.17 mm |
0.0025 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF50 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Thickness 3.17 mm |
0.0025 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF50 L BN047 LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: BeigeInformation.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Thickness 3.17 mm |
0.0025 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF50 L LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: Natural ColorInf.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Thickness 3.17 mm |
0.0025 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF50 RM LE 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables, Low Moisture Absorption and LubricatedInf.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Thickness 3.17 mm |
0.0025 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 GF33 SF L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Strontium FerriteFeatures: LubricatedInformation provided by TP .. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm | 0.0025 in/in | GB/T 15585-1995 |
Sichuan Deyang Haton® hGR30 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP JF004Z PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004Z is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: HV. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.010 cm/cm @Thickness 3.20 mm |
0.0025 - 0.010 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® XP-2140 PPS Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0080 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® XP-2165M PPS Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0080 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® XP-2165MC PPS Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Time 86400 sec |
0.0025 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0030 cm/cm | 0.0025 - 0.0030 in/in | SABIC Method |
SABIC Innovative Plastics NORYL PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0031 cm/cm @Time 86400 sec |
0.0025 - 0.0031 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON EX08318C PEI (Asia Pacific) LNP* Stat-Kon* EX08318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Thickness 6.40 mm |
0.0025 in/in @Thickness 0.252 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+PS LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | on Tensile Bar; ISO 294 |
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Thickness 2.00 mm |
0.0025 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm | 0.0025 in/in | ISO 294-4 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Conditioned, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 cm/cm @Time 86400 sec |
0.0025 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL CN5246 PPE+PS (Asia Pacific) |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
LATI Lastane 50 G/25 PUR, 25% Glass Fiber Reinforced Polyurethane (PUR) based compound. Glass fibers. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Linear Mold Shrinkage, Flow | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
LATI Latilub 80-15T G/30 PPS, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |