SABIC Innovative Plastics LNP THERMOCOMP RF008ESZ PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RF008ESZ PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* RF008ESZ is a compound based on Nylon 6/6 containing 40% Glass Fiber. Added features of this grade include: Easy Molding, Heat Stabilized.
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
Moisture Absorption 0.980 %
0.980 %
50% RH, 24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 92
92
ASTM D785
Tensile Strength at Break 168 MPa
24400 psi
5 mm/min; ISO 527
Tensile Modulus 12.85 GPa
1864 ksi
1 mm/min; ISO 527
Izod Impact, Notched 0.940 J/cm
1.76 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 224 °C
435 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af