Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IRPC Polimaxx Polene G2865 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene G2865 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: HIGH STIFFNESS, GOOD IMPACT STRENGTH, GOOD PROCESSABILITYAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DIARY PRODUCT BOTTLES, FRUIT JUICE BOTTLES, ONE-WAY BOTTLES
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ASTM D792
Environmental Stress Crack Resistance 45 hour
45 hour
Condition B, F50; ASTM D1693
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
1.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
DIN 53505
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 1950 %
1950 %
ASTM D638
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 170 - 200 °C
338 - 392 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved