Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP WF006H PBT (Asia Pacific)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP WF006H PBT (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* WF006H is a compound based on Polybutylene Terephalate resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Time 86400 sec
0.0060 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 119 MPa
17300 psi
ASTM D638
Elongation at Break 2.7 %
2.7 %
ASTM D638
Tensile Modulus 10.44 GPa
1514 ksi
50 mm/min; ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
Flexural Modulus 9.44 GPa
1370 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.13 J/cm
13.4 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
unannealed; ASTM D648