Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp MCR13S PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp MCR13S PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* MCR13S is a compound based on Polypropylene resin containing Carbon Fiber, Barium Sulfate. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
5 mm/min; ISO 527
Elongation at Break 1.0 %
1.0 %
5 mm/min; ISO 527
Flexural Yield Strength 65.0 MPa
9430 psi
2 mm/min; ISO 178
Flexural Modulus 6.30 GPa
914 ksi
2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 20.0 kJ/m²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 131 °C
268 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af