Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp RFB33 PA6.6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp RFB33 PA6.6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP*THERMOCOMP* RFB33 is a compound based on PA66 resin containing Glass Bead, Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 127 MPa
18400 psi
5 mm/min; ISO 527
Elongation at Break 3.0 %
3.0 %
5 mm/min; ISO 527
Tensile Modulus 6.70 GPa
972 ksi
1 mm/min; ISO 527
Flexural Yield Strength 200 MPa
29000 psi
2 mm/min; ISO 178
Flexural Modulus 6.30 GPa
914 ksi
2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 38.0 kJ/m²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 247 °C
477 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
UL 94 by SABIC-IP