Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.70 GPa | 972 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PH 69 GF 30 Polypropylene reinforced with glass fiber Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl.. |
|||
Tensile Modulus | 6.70 GPa @Temperature 150 °C |
972 ksi @Temperature 302 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ASTM D638 |
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ASTM D638 |
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow) |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 35 H2.0 EF 901510 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow) |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | |
LATI Latilub 52/30-15T G/30 PP Homopolymer, 30% Glass Fiber Reinforced Self-lubricating product based on Polypropylene homopolymer (PPh). PTFE. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Tensile Modulus | 6.70 GPa @Temperature 150 °C |
972 ksi @Temperature 302 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ASTM D638 |
Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East) 20% GF Super High Flow PBT |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East) LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP JF004Z PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004Z is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: HV. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1mm/min; ISO 527 |
Teijin Panlite® G-3430H Low Anisotropy, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 30 % of special GF and improved appearance grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPreci.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RFB33 PA6.6 (Europe-Africa-Middle East) LNP*THERMOCOMP* RFB33 is a compound based on PA66 resin containing Glass Bead, Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 6.70 GPa @Temperature 150 °C |
972 ksi @Temperature 302 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-15 S PA6-GF15 Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | D638 |
Ascend Performance Materials VYDYNE® R400G Nylon, Mineral and Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Tensile Modulus | 6.70 GPa @Treatment Temp. 70.0 °C, Time 1.22e+6 sec |
972 ksi @Treatment Temp. 158 °F, Time 340 hour |
62% rel. humidity |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ISO 527-1/-2 |
Lanxess Pocan® KU 2-7209 Z 901510 PBT, 15% Glass Fiber PBT, injection molding grade with 15% glass fibers, elastomer modified, UL 94V0 at 0.8 mm (all colors-in house test), UL-listed from 1.5mm thickness. |
|||
Tensile Modulus | 6.70 GPa | 972 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 3225 Z 000000 PBT, 20% Glass Fiber
(discontinued **) PBT, 20% glass fibers, injection molding, impact modified |