Material Notes:
LNP* Thermotuf* PC006I is a compound based on Nylon 6 resin containing Carbon Fiber, Impact Modifier. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 177 MPa
25700 psi
ASTM D 638
Elongation at Break 2.5 %
2.5 %
ASTM D 638
Tensile Modulus 29.16 GPa
4229 ksi
50 mm/min; ASTM D 638
Flexural Strength 303 MPa
43900 psi
ASTM D 790
Flexural Modulus 15.76 GPa
2286 ksi
ASTM D 790
Izod Impact, Notched 1.97 J/cm

@Temperature 23.0 °C
3.69 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 10.68 J/cm

@Temperature 23.0 °C
20.01 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 208 °C

@Thickness 3.20 mm
406 °F

@Thickness 0.126 in
unannealed; ASTM D 648