Polymer Property : Flexural Modulus = 15.76 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 15.76 GPa
2286 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Stat-kon DEL369E PC
LNP* Stat-Kon* DEL369E is a compound based on Polycarbonate containing Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant and Statically Conductive.This data was supplied by S..
Flexural Modulus 15.76 GPa
2286 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific)
LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 15.76 GPa
2286 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermotuf PC006I PA 6 (Asia Pacific)
LNP* Thermotuf* PC006I is a compound based on Nylon 6 resin containing Carbon Fiber, Impact Modifier. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the..
Flexural Modulus 15.76 GPa
2286 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermotuf PC006I PA 6
LNP* Thermotuf* PC006I is a compound based on Nylon 6 resin containing Carbon Fiber, Impact Modifier. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the..