Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.76 GPa | 2286 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC LNP* Stat-Kon* DEL369E is a compound based on Polycarbonate containing Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant and Statically Conductive.This data was supplied by S.. |
|||
Flexural Modulus | 15.76 GPa | 2286 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific) LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 15.76 GPa | 2286 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermotuf PC006I PA 6 (Asia Pacific) LNP* Thermotuf* PC006I is a compound based on Nylon 6 resin containing Carbon Fiber, Impact Modifier. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the.. |
|||
Flexural Modulus | 15.76 GPa | 2286 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermotuf PC006I PA 6 LNP* Thermotuf* PC006I is a compound based on Nylon 6 resin containing Carbon Fiber, Impact Modifier. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the.. |