SABIC Innovative Plastics LNP VERTON MV00ASXC PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON MV00ASXC PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* VERTON* MV00ASXC is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 118 MPa
17100 psi
5 mm/min; ISO 527
Elongation at Break 1.6 %
1.6 %
5 mm/min; ISO 527
Tensile Modulus 11.3 GPa
1640 ksi
1 mm/min; ISO 527
Flexural Strength 180 MPa
26100 psi
2 mm/min; ISO 178
Flexural Modulus 10.1 GPa
1460 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C
325 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
315 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94