Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 21.0 kJ/m² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific) Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML7681 PC Copolymer (Asia Pacific) Polycarbonate with high flow, good processability, good impact and thermal properties, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited translucent colors onl.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 10.0 ft-lb/in² | ASTM D256 |
Ineos K38-20-160 Polyethylene Copolymer K38-20-160 is a medium density polyethylene copolymer containing an organic yellow pigment system, designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stres.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, Conditioned Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, Conditioned Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer (Europe-Africa-Middle East) LNP* LUBRICOMP* YL003 is a compound based on Polyester Elastomer containing PTFE. Added features include; Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON DX11408 PC LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific) LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS (Asia Pacific) LNP* Verton* NV003E is a compound based on PC+ABS Blend resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA High flow PPO+PA. Power distribution box applications. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11 LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV00ASXC PP (Europe-Africa-Middle East) LNP* VERTON* MV00ASXC is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East) Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating .. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | Conditioned; ISO 180/1A |
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6 Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DSM Arnitel® PL650 Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-717C ABS Medium impact |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 + Polyamide 6 Zytel 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was develop.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | ISO Test |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl C2 V30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 21.0 kJ/m² | 9.99 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics GELOY XP4025 ASA+PC Available in a wide range of colors and is recommended for unpainted exterior applications. |