SABIC Innovative Plastics LNP VERTON RV0079 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RV0079 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing Flame Retardant, Long Glass Fiber, Long Glass. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.69 g/cc
0.0611 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 213 MPa
30900 psi
ISO 527
Elongation at Break 1.8 %
1.8 %
ISO 527
Tensile Modulus 15.07 GPa
2186 ksi
1 mm/min; ISO 527
Flexural Strength 298 MPa
43200 psi
ISO 178
Flexural Modulus 13.28 GPa
1926 ksi
ISO 178
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 57.0 kJ/m²
27.1 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 262 °C
504 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 259 °C
498 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.70 mm
V-0

@Thickness 0.0669 in
UL 94 by SABIC-IP