Polymer Property : Izod Impact, Notched (ISO) = 32.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS
Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press.
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer
PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East)
11 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4mm, Cut; ISO 180/1A
SABIC Innovative Plastics SABIC PPCOMPOUND 9712 PP
SABIC® PPcompound 9712 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st..
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS
LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t..
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific)
LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t..
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific)
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 (Asia Pacific)
LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing Flame Retardant, Long Glass Fiber, Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
ISO 180/1A
Borealis Daplen™ EG203AE Polypropylene Compound Elastomer and Mineral Modified
Daplen EG203AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EG203AE is a material with excellent impact /stiffness ratio. Thanks to its low ..
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -50.0 °C
15.2 ft-lb/in²

@Temperature -58.0 °F
Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene
Next Generation DOWLEX® IP-2580 resin is an improved processing linear low density polyethylene resin designed for excellent flow and stiffness with freezer grade impact properties. DOWLEX IP-2580 ..
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -50.0 °C
15.2 ft-lb/in²

@Temperature -58.0 °F
Dow LDPE 993I Low Density Polyethylene
DOW LDPE 993I resin is a low slip, medium molecular weight distribution homopolymer designed to offer good gloss and rigidity with excellent flow characteristics. This resin has good processability ..
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
ISO 180/A
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned)
Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity.
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature 23.0 °C
15.2 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned)
Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas..
Izod Impact, Notched (ISO) 32.0 kJ/m²
15.2 ft-lb/in²
Conditioned; ISO 180/1A
Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled
Glass fiber reinforced, high resistance to frictionInformation provided by Addiplast.
Izod Impact, Notched (ISO) 32.0 kJ/m²

@Temperature -30.0 °C
15.2 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East)
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only