SABIC Innovative Plastics LNP VERTON RX07013 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RX07013 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP VERTON * RX07013 is a compound based on Nylon 66 resin containig Long Glass. Added features of this material include: Easy Molding and UV Resistant.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 265 MPa
38400 psi
5 mm/min; ISO 527
Elongation at Break 1.9 %
1.9 %
5 mm/min; ISO 527
Tensile Modulus 18.38 GPa
2666 ksi
1 mm/min; ISO 527
Flexural Modulus 15.55 GPa
2255 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1A
38.0 kJ/m²

@Temperature -40.0 °C
18.1 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 89.0 kJ/m²
42.4 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 67.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 258 °C
496 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
487 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af