Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Verton UV007S PPA (Asia Pacific)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Verton UV007S PPA (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP VERTON* UV007S is a compound based on Polyphthalamide resin containing Long Glass, Long Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 181 MPa
26300 psi
ISO 527
Elongation at Break 1.6 %
1.6 %
ISO 527
Tensile Modulus 12.5 GPa
1810 ksi
1 mm/min; ISO 527
Flexural Strength 265 MPa
38400 psi
ISO 178
Flexural Modulus 11.2 GPa
1620 ksi
ISO 178
Izod Impact, Notched (ISO) 23.0 kJ/m²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af