Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.2 GPa | 1620 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
LNP Lubricomp® PDX-U-95672 BK8-115 Polyphthalamide, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF40 HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF40 HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF40 UV L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceAppearan.. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
Techmer ES HiFill® PPA GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | GB/T 9341-2008 |
Sichuan Deyang Haton® hGR31M1 Polyphenylene Sulfide Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF40 FR HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Flexural Modulus | 11.2 GPa | 1630 ksi | ASTM D 790 |
RTP Company RTP 2099 X 121249 C Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 68% Renewable Resource Content Nucleated for high heat exposure. For detailed processing information regarding this, see the PLA Molding Guide on the RTP Company website. This material has received the "USDA Certified Biob.. |
|||
Flexural Modulus | 11.2 GPa | 1630 ksi | ASTM D 790 |
RTP Company RTP 2099 X 126216 C Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 68% Renewable Resource Content Nucleated for high heat exposure. For detailed processing information regarding this, see the PLA Molding Guide on the RTP Company website. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
E-Polymers SEPAZ® N6030FR 30% Glass Fiber Reinforced Flame Retardant Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, Conditioned Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, Conditioned Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 446 Glass/Mineral Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 441 Glass Reinforced, PET Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.32% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ISO Value |
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is .. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ISO 178 |
SABIC Innovative Plastics LNP Verton UV007S PPA LNP VERTON* UV007S is a compound based on Polyphthalamide resin containing Long Glass, Long Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP .. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ISO 178 |
SABIC Innovative Plastics LNP Verton UV007S PPA (Asia Pacific) LNP VERTON* UV007S is a compound based on Polyphthalamide resin containing Long Glass, Long Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP .. |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM-D790 |
Polyram Polytron A40N02 Nylon 66, 40% Long Fiber 40% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 11.2 GPa | 1630 ksi | ASTM D 790 |
RTP Company RTP 2383 A Rigid Thermoplastic Polyurethane (RTPU), Carbon Fiber |
|||
Flexural Modulus | 11.2 GPa | 1620 ksi | ASTM-D790 |
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |