Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstability under heat exposure. Developed for lightguide and LED applicatons. It meets WEEE/RoHS requirements for various applications.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Moisture Absorption 0.150 %
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %
0.35 %
ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0060 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 7.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.0 MPa
8410 psi
50 mm/min; ISO 527
65.0 MPa
9430 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa
8990 psi
Type I, 50 mm/min; ASTM D638
62.0 MPa
8990 psi
50 mm/min; ISO 527
Elongation at Break 77 %
77 %
50 mm/min; ISO 527
85 %
85 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
Type I, 50 mm/min; ASTM D638
6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 2.23 GPa
323 ksi
1 mm/min; ISO 527
2.30 GPa
334 ksi
5 mm/min; ASTM D638
Flexural Strength 95.0 MPa
13800 psi
12.5 mm/min; ISO 178
Flexural Yield Strength 95.0 MPa
13800 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
1.3 mm/min, 50 mm span; ASTM D790
2.25 GPa
326 ksi
2 mm/min; ISO 178
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*3; ISO 180/1A
18.0 kJ/m²

@Temperature -30.0 °C
8.57 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
Dart Drop, Total Energy 70.0 J

@Temperature 23.0 °C
51.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
125 °C

@Thickness 3.20 mm
257 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 142 °C
288 °F
Rate B/50; ASTM D1525
145 °C
293 °F
Rate B/120; ISO 306
UL RTI, Electrical 125 °C
257 °F
UL 746B
UL RTI, Mechanical with Impact 115 °C
239 °F
UL 746B
UL RTI, Mechanical without Impact 125 °C
257 °F
UL 746B
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
Glow Wire Test 850 °C
1560 °F
IEC 60695-2-13
850 °C
1560 °F
IEC 60695-2-13
960 °C

@Thickness 1.00 mm
1760 °F

@Thickness 0.0394 in
IEC 60695-2-12
Optical Properties Metric English Comments
Refractive Index 1.586
1.586
ISO 489
Haze 1.0 %

@Thickness 2.00 mm
1.0 %

@Thickness 0.0787 in
SABIC Method
Transmission, Visible >= 88 %
>= 88 %
2.54 mm, 420nm; SABIC Method
>= 90 %
>= 90 %
2.54 mm; ASTM D1003
Electrical Properties Metric English Comments
Comparative Tracking Index 175 - 250 V
175 - 250 V
UL 746A
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
60 - 120 arcs
UL 746A
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved