Material Notes:
Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets. MFR of 25.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 25 g/10 min

@Load 1.20 kg,
Temperature 300 °C
25 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 110 %
110 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 93.0 MPa
13500 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Dart Drop, Total Energy 54.0 J
39.8 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 126 °C

@Thickness 6.40 mm
259 °F

@Thickness 0.252 in
unannealed; ASTM D648