Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HF1110 PC General purpose grade. Good clarity, heat resistance, property retention and dimensional stability. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HF1130R PC PC, High Flow, Mold Release, UV-Stabilized |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HF1140R PC High flow grade. Heat stabilized. Enhanced level of mold release. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported with biocompatib.. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HPS1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® LSHF PC (Asia Pacific) Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® LSHF PC (Europe-Africa-Middle East) Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® OQ3120 PC High Flow. UV-stabilized. Inherent mold release. Ophthalmic lenses. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS High impact and ductility at 73F and -20F. For thin-wall applications. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Suitable for thin wall application. Low temperature ductility (-20F). For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature -30.0 °C |
39.8 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HF1110R PC (Asia Pacific) High flow grade. Easy mold release version of LEXAN HF1110. For thin wall lighting lenses, data storage components and safety eyewear lenses. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HF1130 PC (Asia Pacific) UV-stabilized. Good clarity, heat resistance, property retention and dimensional stability. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HF1140 PC Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this.. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Asia Pacific) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL HNA055 PPE+HIPS (Europe-Africa-Middle East) >PPE+PS-HI< Autoclavable engineering thermoplastic. Biocompatible per ISO10993 (color dependent). |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Dart Drop, Total Energy | 54.0 J @Temperature 23.0 °C |
39.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® V2000DM PBT Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Dart Drop, Total Energy | 54.0 J | 39.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® HF1110 PC (Asia Pacific) General purpose grade. Good clarity, heat resistance, property retention and dimensional stability. |