Material Notes:
Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 8.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
8.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
Type I, 50 mm/min; ASTM D638
Elongation at Yield 130 %
130 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 97.0 MPa
14100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 7.47 J/cm
14.0 ft-lb/in
ASTM D256
Dart Drop, Total Energy 169 J
125 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C

@Thickness 6.40 mm
270 °F

@Thickness 0.252 in
unannealed; ASTM D648