SABIC Innovative Plastics NORYL INT1512 PPE+HIPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL INT1512 PPE+HIPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE/HIPS GF filled for auto interior
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0060 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 39.3 g/10 min

@Load 10.0 kg,
Temperature 250 °C
39.3 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
SABIC - Japan Method
Elongation at Break 10 %
10 %
SABIC - Japan Method
Flexural Strength 101 MPa
14600 psi
ASTM D790
Flexural Modulus 3.82 GPa
554 ksi
ASTM D790
Izod Impact, Notched 0.980 J/cm
1.84 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
27.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 6.40 mm
244 °F

@Thickness 0.252 in
unannealed; ASTM D648