Physical Properties Metric English Comments
Melt Flow 39.3 g/10 min

@Load 10.0 kg,
Temperature 250 °C
39.3 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL INT1512 PPE+HIPS (Asia Pacific)
PPE/HIPS GF filled for auto interior
Melt Flow 39.3 g/10 min

@Load 5.00 kg,
Temperature 275 °C
39.3 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Melt Flow 39.3 g/10 min

@Load 5.00 kg,
Temperature 275 °C
39.3 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Dry)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Melt Flow 39.3 g/10 min

@Load 5.00 kg,
Temperature 275 °C
39.3 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Melt Flow 39.3 g/10 min

@Load 5.00 kg,
Temperature 275 °C
39.3 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Dry)