Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL NH5110E PPE+PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL NH5110E PPE+PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NORYL NH5110E is a flame retardant, non halogenated, impact modified extrusion grade. Developed for low beard-growth, with a Vicat B/120 of 138 Deg C, according to ISO 306 and a UL-94 rating of V1@ 1.5mm, it would be suitable for electrical conduit and cable management applications.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Moisture Absorption 0.0600 %
0.0600 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.15 %
0.15 %
ISO 62
Melt Index of Compound 9.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 52.0 MPa
7540 psi
50 mm/min; ISO 527
Tensile Strength, Yield 64.0 MPa
9280 psi
50 mm/min; ISO 527
Elongation at Break 18 %
18 %
50 mm/min; ISO 527
Elongation at Yield 4.0 %
4.0 %
50 mm/min; ISO 527
Tensile Modulus 2.50 GPa
363 ksi
1 mm/min; ISO 527
Flexural Yield Strength 98.0 MPa
14200 psi
2 mm/min; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 24.0 kJ/m²
11.4 ft-lb/in²
80*10*4; ISO 180/1A
9.00 kJ/m²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.60 J/cm²
12.4 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 82.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
45.6 µin/in-°F

@Temperature 73.4 - 176 °F
ASTM E 831
82.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
45.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
52.2 µin/in-°F

@Temperature 73.4 - 176 °F
ASTM E 831
94.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
52.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
264 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 114 °C
237 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 138 °C
280 °F
Rate B/120; ISO 306
149 °C
300 °F
Rate B/50; ISO 306
UL RTI, Electrical 65.0 °C
149 °F
UL 746B
UL RTI, Mechanical with Impact 65.0 °C
149 °F
UL 746B
UL RTI, Mechanical without Impact 65.0 °C
149 °F
UL 746B
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
UL 94
Oxygen Index 34 %
34 %
ISO 4589
Electrical Properties Metric English Comments
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
ASTM D150
2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 46.0 kV/mm

@Thickness 1.00 mm
1170 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
Dissipation Factor 0.0017

@Frequency 1.00e+6 Hz
0.0017

@Frequency 1.00e+6 Hz
ASTM D150
0.0017

@Frequency 1.00e+6 Hz
0.0017

@Frequency 1.00e+6 Hz
IEC 60250
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C Pass
IEC 60695-10-2