Material Notes:
PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. FDA 21CFR177.1660 compliant. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Water Absorption 0.080 %

@Time 86400 sec
0.080 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0090 - 0.016 cm/cm

@Thickness 0.750 - 2.30 mm
0.0090 - 0.016 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
0.015 - 0.023 cm/cm

@Thickness 2.30 - 4.60 mm
0.015 - 0.023 in/in

@Thickness 0.0906 - 0.181 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.010 - 0.017 cm/cm

@Thickness 0.750 - 2.30 mm
0.010 - 0.017 in/in

@Thickness 0.0295 - 0.0906 in
SABIC Method
0.016 - 0.024 cm/cm

@Thickness 2.30 - 4.60 mm
0.016 - 0.024 in/in

@Thickness 0.0906 - 0.181 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.0 MPa
8120 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 17.9 %
17.9 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 84.0 MPa
12200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.39 GPa
347 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 18.5 J/cm
34.7 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 81.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 128 °C

@Thickness 6.40 mm
262 °F

@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C

@Thickness 6.40 mm
120 °F

@Thickness 0.252 in
unannealed; ASTM D648
Descriptive Properties Value Comments
Specific Volume 0.76cm^3/g
ASTM D792