Polymer Property : CTE, linear, Parallel to Flow = 139 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific)
Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 195 PBT
PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 195HP PBT
PELLET FORM. For compounding only (not for injection molding). Unreinforced PBT. FDA 21CFR177.1660 compliant. Melt viscosity between 740 and 900 poise. Natural Color (1001) Only.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 215HPR PBT
Unreinforced PBT with mold release. FDA food contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility data. Alternative grade Valox HX21..
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 295 PBT
Unreinforced PBTThis data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 310 PBT
Unreinforced, general purpose. Typical viscosity 5000-7000.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific)
Unreinforced, general purpose. Typical viscosity 5000-7000.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 310HP PBT
PBT for compounding/fibers only. Not intended for injection molding. FDA compliant. Available in Natural color (1001) only.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 311 PBT
Unreinforced, improved resistance to UV. Medium viscosity.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 312 PBT
Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific)
Unreinforced, For compounding only (not for injection molding), Medium viscosity.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 315 PBT
Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 325 PBT
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific)
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 745 PBT
30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks.
CTE, linear, Parallel to Flow 139 µm/m-°C

@Temperature 60.0 - 138 °C
77.2 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific)
30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks.