Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SCG Chemicals EL-Leneâ„¢ LD1630J Low Density Polyethylene Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ LD1630J Low Density Polyethylene Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics:Good flowability for multicavitiesGood toughness and flexibilityExcellent gloss and transparencyOdorlessSafe for food contactRecommended Applications:HousewaresSmall to large closuresBase resin for powder coating applicationToy partsMasterbatch carrierInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.916 g/cc
0.916 g/cc
ASTM D1505
Linear Mold Shrinkage, Flow 0.0223 cm/cm

@Thickness 2.00 mm
0.0223 in/in

@Thickness 0.0787 in
TPE Method
Linear Mold Shrinkage, Transverse 0.0167 cm/cm

@Thickness 2.00 mm
0.0167 in/in

@Thickness 0.0787 in
TPE Method
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ASTM D2240
Tensile Strength at Break 9.00 MPa
1310 psi
ASTM D638
Tensile Strength, Yield 8.83 MPa
1280 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Flexural Modulus 0.167 GPa
24.2 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 105 °C
221 °F
ASTM D2117
Vicat Softening Point 85.0 °C
185 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 14 %

@Thickness 1.00 mm
14 %

@Thickness 0.0394 in
ASTM D1003
Gloss 76 %

@Thickness 1.00 mm
76 %

@Thickness 0.0394 in
ASTM D2457
Users viewing this material also viewed the following: