SCG Chemicals EL-Leneâ„¢ M10 Butene (C4) Rotational Molding Resin

Category Polymer , Thermoplastic
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ M10 Butene (C4) Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Color compound resin available in pellet / powder formKey Characteristics:High stiffnessGood processingFair impact resistanceTypical Applications: General-purpose products, such as small-to-medium water tanks (
Physical Properties Metric English Comments
Specific Gravity 0.938 g/cc
0.938 g/cc
ASTM D1505
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D368
Flexural Modulus 0.700 GPa
102 ksi
ASTM D790
Dart Drop Total Energy 1.90 J/cm

@Thickness 5.00 mm,
Temperature -40.0 °C
0.00356 ft-lb/mil

@Thickness 0.197 in,
Temperature -40.0 °F
ARM Method
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
ASTM D2117
Crystallization Temperature 113 °C
235 °F
ASTM D2117
Descriptive Properties Value Comments
Food Contact Approved FDA
Heavy Metal Free (Base Resin) Yes
Peak Internal Air Temperature 195°C
TPE Method
Shrinkage Level medium
TPE Method
UV Stabilizer UV-8 & Low UV
ASTM G155