S&E Specialty Polymers TufTech™ GA-3188AHP PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ GA-3188AHP PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: RoHS compliant, phthalate free, 105°C flame retardant jacketing material suitable for extrusion applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 88.0

@Time 15.0 sec
88.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 19.3 MPa
2800 psi
ASTM D412
20.458 MPa

@Temperature 100 °C,
Time 14400 sec
2967.2 psi

@Temperature 212 °F,
Time 4.00 hour
Oil Aged
Elongation at Break 300 %
300 %
ASTM D412
>= 234 %

@Treatment Temp. 100 °C,
Time 14400 sec
>= 234 %

@Treatment Temp. 212 °F,
Time 4.00 hour
Oil Aged
Abrasion 80.0

@Load 1.00 kg
80.0

@Load 2.20 lb
Taber, H18 Wheel; ASTM D4060
Thermal Properties Metric English Comments
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Oxygen Index 27.5 %
27.5 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 174 - 185 °C
345 - 365 °F
Suggested Stock