Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ASTM D2240
Tensile Strength, Ultimate 53.9 MPa
7820 psi
ASTM D638
Tensile Strength, Yield 20.6 MPa

@Strain 5.00 %
2990 psi

@Strain 5.00 %
ASTM D638
27.5 MPa

@Strain 10.0 %
3980 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Flexural Modulus 0.490 GPa
71.1 ksi
ASTM D790
Tear Strength 190 kN/m
1080 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ASTM D648