Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 190 kN/m | 1080 pli | DIN 53.517 |
Lubrizol Advanced Materials Pearlthane® Clear 15N60D Thermoplastic Polyurethane
(discontinued **) Polyester-based TPU, supplied in form of translucent, colorless or slightly yellowish pellets, combining very high hardness with excellent mechanical properties and excellent hyrdrolysis resistance... |
|||
Tear Strength | 190 kN/m | 1080 pli | ISO 34-1B |
Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining high hardness with excellent mechanical properties and .. |
|||
Tear Strength | 189 kN/m | 1080 pli | Die C; ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |
|||
Tear Strength | 190 kN/m | 1080 pli | ASTM D1004 |
SK Chemicals SKYPEL M572CR Special Grade Copper Resistance SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tear Strength | >= 190 kN/m | >= 1080 pli | ISO 34 |
Austin Novel Materials Texalan® 472D Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tear Strength | 190 kN/m | 1080 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR6520 Standard Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |