Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SPS Guang Zhou SAMATâ„¢ EP 5001(f1) Flame-retarded Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer SPS Guang Zhou
Trade Name SAMAT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou SAMATâ„¢ EP 5001(f1) Flame-retarded Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristic: Good flame retardance, non-halogen, high flow properties, high rigidity, high heat resistance, meets the requirements of RoHs and PaHs, excellent UV resistanceApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Flexural Strength 40.0 MPa
5800 psi
Flexural Modulus 2.50 GPa
363 ksi
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
ASTM D648
Descriptive Properties Value Comments
Flammability UL1694-SC-0