Saint-Gobain Chemfab® 14 Porous PTFE-Coated Glass

Category Ceramic , Glass , Glass Fiber
Manufacturer Saint-Gobain Quartz PLC
Trade Name Chemfab®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Chemfab® 14 Porous PTFE-Coated Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas." All data based on a 0.011 inch test sample. Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Mechanical Properties Metric English Comments
Tear Strength Test 275
275
Lbs./In. Propagation Tear Strength in fill/transverse direction
325
325
Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 30.7 kN/m
175 pli
Tensile Strength (Fill)
39.4 kN/m
225 pli
Tensile Strength (Warp)
Descriptive Properties Value Comments
Weight (oz/yd^2) 9.9