Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Fluoroloy® A22 High Performance Seal Material

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Fluoroloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Fluoroloy® A22 High Performance Seal Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High modulus with excellent high-temperature resistance; Abrasion resistant; Chemically Inert; Recommended for back-up rings and for special applications. Information provided by Saint-Gobain Performance Plastics.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Deformation 0.030 %

@Time 86400 sec
0.030 %

@Time 24.0 hour
13.8 MPa (2000 psi) load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
ASTM D2240
Tensile Strength 95.0 MPa
13800 psi
ASTM D4894
Elongation at Break 30 %
30 %
ASTM D4894
Tensile Modulus 4.00 GPa
580 ksi
ASTM D4894
Compressive Yield Strength 138 MPa

@Strain 1.00 %
20000 psi

@Strain 1.00 %
ASTM D695
Compressive Modulus 2.441 GPa
354.0 ksi
ASTM D695
Coefficient of Friction 0.40
0.40
Saint-Gobain Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 55.6 µm/m-°C

@Temperature 26.0 - 200 °C
30.9 µin/in-°F

@Temperature 78.8 - 392 °F
Mold Direction; ASTM D696
CTE, linear, Transverse to Flow 78.5 µm/m-°C

@Temperature 26.0 - 200 °C
43.6 µin/in-°F

@Temperature 78.8 - 392 °F
ASTM D696
Maximum Service Temperature, Air 260 °C
500 °F
Descriptive Properties Value Comments
Color Tan
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved