Saint-Gobain Rulon® 125 Bearing/Seal PTFE

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Rulon® 125 Bearing/Seal PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Rulon 125 is used primarily in applications that are not severe such as dryer drum slides and piston rings in pneumatic or hydraulic controls.Information provided by distributor TriStar Plastics Corp.
Physical Properties Metric English Comments
Density 2.09 g/cc
0.0755 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength, Yield 10.3 MPa
1500 psi
Elongation at Break 60 %
60 %
Tensile Modulus 1.59 GPa
230 ksi
Flexural Modulus 1.38 GPa
200 ksi
Izod Impact, Notched 3.20 J/cm
6.00 ft-lb/in
Coefficient of Friction, Dynamic 0.012
0.012
Dry vs. Steel
Coefficient of Friction, Static 0.018
0.018
Dry vs. Steel
Thermal Properties Metric English Comments
Thermal Conductivity 0.648 W/m-K
4.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C
550 °F
Continuous
316 °C
600 °F
Short Term
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 2.65

@Frequency 1.00e+6 Hz
2.65

@Frequency 1.00e+6 Hz
Dielectric Strength 14.8 kV/mm
375 kV/in
Short Term
Descriptive Properties Value Comments
Color Black