Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Melt Flow 32.4 g/10 min

@Load 10.0 kg,
Temperature 250 °C
32.4 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 55.9 MPa
8110 psi
50 mm/min; ASTM D638
Flexural Strength 76.5 MPa
11100 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 7.06 J/cm

@Thickness 3.17 mm
13.2 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C

@Thickness 6.40 mm
225 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 131 °C
268 °F
B/50; ISO R306