Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific) 7 MFR LEXAN HFD Copolymer |
|||
Vicat Softening Point | 131 °C | 268 °F | 50°C/hr; 50N |
Polimeri Europa KOBLEND HI 20 PBT+PC, Impact Grade
(discontinued **) PBT elastomer modified with good impact behaviour, good stiffness, resistant to solvents. Main application fields: automotive industryUnfilled. Suitable for Injection Molding. Supplied as pellets.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer 7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer 7 MFR LEXAN HFD Copolymer |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Vicat Softening Point | 131 °C | 268 °F | 50°C/h 50N; ISO 306 |
LATI LATILUB 73/13-20ST Polyoxymethylene Base (POM), 20% Mixed PTFE/Silicone Self Lubricating Plastic
(discon Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Vicat Softening Point | 131 °C | 268 °F | 50°C/h 50N; ISO 306 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
Ineos B54-25H-127 HDPE B54-25H-127 is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmenta.. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
LyondellBasell Petrothene® LB832001 High Density Polyethylene ApplicationsPETROTHENE LB 8320-00 resin is designed for sheet extrusion, vacuum forming and thermoforming. This resin exhibits very low sag, high stiffness.Regulatory StatusLB 8320-00 meets the req.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 131 °C | 268 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 131 °C | 268 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 131 °C | 268 °F | 50N / 50°C/hr; ISO 306B |
Styron Pulse® 979 PC/ABS PULSE™ 979 is a high performance, 10% glass filled PC/ABS resin.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP High modulus/impact/heat PPE+PP |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X5601WX PBT + PC + PET Impact modified PBT+PC+PET, Heat aging improved Xenoy |
|||
Vicat Softening Point | 131 °C | 268 °F | 50N; ISO 306 |
Denka MALECCA K-510 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
ExxonMobil Paxon™ FD60-018 Compression Molding Resin FD60-018 is a very high molecular weight high density polyethylene powder. It exhibits very high impact strength.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate A, Loading 1 (10 N); ASTM D1525 |
Entec Hypel® PEHD10/.964 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
Dow DMDA-8007 NT 7 High Density Polyethylene Resin DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin .. |
|||
Vicat Softening Point | 131 °C | 268 °F | |
Covestro Bayblend® KL 1-1427 Polycarbonate/ABS Blend Glass fiber reinforced grade (30%) with high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
Vicat Softening Point | 131 °C @Load 1.00 kg, Thickness 3.17 mm |
268 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ASA TW18B3 ASA Weatherable Polymers Injection Molding Grade, Very High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
Dow UNIVAL™ DMDH-6400 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDH-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, water and fruit drinks. In a.. |
|||
Vicat Softening Point | 131 °C @Load 1.02 kg |
268 °F @Load 2.25 lb |
ISO 306 |
Arkema Group Pebax® 4033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Vicat Softening Point | 131 °C @Load 1.02 kg |
268 °F @Load 2.25 lb |
ISO 306 |
Arkema Group Pebax® 4033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Vicat Softening Point | 131 °C | 268 °F | B/120; ISO R306 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |