Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 131 °C @Load 1.00 kg |
268 °F @Load 2.20 lb |
Rate B; 120°C/min; ASTM D 1525 |
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn.. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D 1525 |
NOVA Chemicals Novapol® HE-W959-A HDPE Extrusion/Blow Molding Resin HE-W959-A complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food. It is also biolog.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East) XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® EXRL0683 PC Copolymer 11 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
Chevron Phillips HiD® 9706 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: moderate flow, good impact strength, excellent stiffness, good ESCR, moderate shrinkage resistanceApplications: crates and totes, structural foamInform.. |
|||
Vicat Softening Point | 131 °C | 268 °F | 50°C/h 50N; ISO 306 |
LATI LATILUB 73/13-20ST Polyoxymethylene Base (POM), 20% Mixed PTFE/Silicone Self Lubricating Plastic
(discon Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Vicat Softening Point | 131 °C | 268 °F | 50°C/h 50N; ISO 306 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
Ineos G60-25-144 HDPE Ineos G60-25-144 is a high density polyethylene homopolymer typically used in the production of sheet extrusion and blow molded containers. This material meets the Food and Drug Administration requ.. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
Ineos T50-200 HDPE Ineos T50-200 is a high density polyethylene copolymer of narrow molecular weight distribution. It is intended for injection molding applications which require high impact resistance and good envir.. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
LyondellBasell Petrothene® LB832001 High Density Polyethylene ApplicationsPETROTHENE LB 8320-00 resin is designed for sheet extrusion, vacuum forming and thermoforming. This resin exhibits very low sag, high stiffness.Regulatory StatusLB 8320-00 meets the req.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 131 °C | 268 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 131 °C | 268 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® AE-2030 PC/PET, General Purpose PC/PET material used for automobile radiator grills and door handlesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Vicat Softening Point | 131 °C | 268 °F | 50N; ISO 306 |
Denka MALECCA K-510 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
ExxonMobil Paxon™ FD60-018 Compression Molding Resin FD60-018 is a very high molecular weight high density polyethylene powder. It exhibits very high impact strength.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 131 °C | 268 °F | ASTM D1525 |
Dow DMDA-8007 NT 7 High Density Polyethylene Resin DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin .. |
|||
Vicat Softening Point | 131 °C @Load 1.00 kg, Thickness 3.17 mm |
268 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ASA TW18B3 ASA Weatherable Polymers Injection Molding Grade, Very High Heat Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 131 °C @Load 1.02 kg |
268 °F @Load 2.25 lb |
ISO 306 |
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Vicat Softening Point | 131 °C @Load 1.02 kg |
268 °F @Load 2.25 lb |
ISO 306 |
Arkema Group Pebax® 4033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Vicat Softening Point | 131 °C | 268 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Vicat Softening Point | 131 °C | 268 °F | B/120; ISO R306 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |