Samsung Cheil Industries Infino® GW-1041 PC/ABS, Unreinforced Recycled

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® GW-1041 PC/ABS, Unreinforced Recycled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 19 g/10 min

@Load 10.0 kg,
Temperature 250 °C
19 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 52.0 MPa
7540 psi
50 mm/min; ASTM D638
Flexural Strength 74.5 MPa
10800 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.96 GPa
284 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 6.86 J/cm

@Thickness 3.17 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C

@Thickness 6.40 mm
250 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 138 °C
280 °F
B/50; ISO R306