Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® HN-1064IA PC, Unreinforced FR

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® HN-1064IA PC, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Melt Flow 17 g/10 min

@Load 10.0 kg,
Temperature 250 °C
17 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Yield 56.9 MPa
8250 psi
50 mm/min; ASTM D638
Flexural Strength 77.5 MPa
11200 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.67 GPa
242 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 6.37 J/cm

@Thickness 6.35 mm
11.9 ft-lb/in

@Thickness 0.250 in
ASTM D256
7.35 J/cm

@Thickness 3.17 mm
13.8 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 143 °C
289 °F
B/50; ISO R306
UL RTI, Electrical 130 °C
266 °F
UL RTI, Mechanical with Impact 130 °C
266 °F
UL RTI, Mechanical without Impact 130 °C
266 °F
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
V-0

@Thickness 1.50 - 3.00 mm
V-0

@Thickness 0.0591 - 0.118 in