Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 26 g/10 min

@Load 10.0 kg,
Temperature 220 °C
26 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Yield 63.7 MPa
9250 psi
50 mm/min; ASTM D638
Flexural Strength 88.3 MPa
12800 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 5.39 J/cm

@Thickness 3.17 mm
10.1 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C

@Thickness 6.40 mm
198 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 103 °C
217 °F
B/50; ISO R306
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
5VB

@Thickness 3.00 mm
5VB

@Thickness 0.118 in
5VA

@Thickness 2.50 mm
5VA

@Thickness 0.0984 in