Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.39 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
10.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical |
|||
Izod Impact, Notched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
Haysite H258 Polyester Laminate Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications.. |
|||
Izod Impact, Notched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
Haysite H260 Polyester Laminate Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet m.. |
|||
Izod Impact, Notched | 5.41 J/cm | 10.1 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin.. |
|||
Izod Impact, Notched | 5.39 J/cm @Thickness 3.17 mm |
10.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.39 J/cm @Thickness 3.17 mm |
10.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.39 J/cm @Thickness 3.17 mm |
10.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1014S PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.39 J/cm @Thickness 3.17 mm |
10.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.39 J/cm @Thickness 3.17 mm |
10.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 210NHF Polymer Alloy, Flame Retardancy (Non-Halogen) Excellent impact, formability and weather resistance.210NHF is a flame retardant (non-halogen) grade.Applications: LCD TV Rear Cover (high flow)Information provided by Samyang. |
|||
Izod Impact, Notched | 5.39 J/cm | 10.1 ft-lb/in | 1/8 in. notch; ASTM D256 |
CPC - Vycom FLAMETEC™ CP7-D Flame Retardant Polypropylene Flametec™ CP7-D is a proprietary designation for a flame retardant polypropylene formulation. CP7-D represent our version of polypropylene sheet whose flame retardant characteristics meet or exceed.. |
|||
Izod Impact, Notched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Izod Impact, Notched | 5.40 J/cm @Thickness 3.17 mm |
10.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers DIAMALOY XNY-1012U Polycarbonate/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 5.40 J/cm @Thickness 3.17 mm |
10.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers PC 2418 R UV UV Stabilized/Mold Release Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |