Samsung Cheil Industries Infino® XK-2307 PPS

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® XK-2307 PPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Thickness 3.20 mm
0.0010 in/in

@Thickness 0.126 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 cm/cm

@Thickness 3.20 mm
0.0030 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 330 °C
15 g/10 min

@Load 11.0 lb,
Temperature 626 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Flexural Strength 118 MPa
17100 psi
2.8 mm/min; ASTM D638
Flexural Modulus 17.7 GPa
2560 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 0.441 J/cm

@Thickness 3.17 mm
0.827 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 270 °C

@Thickness 6.40 mm
>= 518 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
V-0

@Thickness 2.00 - 3.00 mm
V-0

@Thickness 0.0787 - 0.118 in
Users viewing this material also viewed the following: