Polymer Property : Specific Gravity = 1.70 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.70 - 1.85 g/cc
1.70 - 1.85 g/cc
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Specific Gravity 1.70 - 1.85 g/cc
1.70 - 1.85 g/cc
Premix Premi-Glas® 1200H-20 Polyester SMC
Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec..
Specific Gravity 1.70 - 1.85 g/cc
1.70 - 1.85 g/cc
Premix Premi-Glas® 2103-22 CR-SX-HT Fiberglass Reinforced Thermoset BMC
Premi-Glas® 2103-22 CR-SX-HT is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL ..
Specific Gravity 1.70 - 1.80 g/cc
1.70 - 1.80 g/cc
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound
Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
Specific Gravity 1.70 - 1.85 g/cc
1.70 - 1.85 g/cc
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Specific Gravity 1.70 - 1.85 g/cc
1.70 - 1.85 g/cc
Premix Premi-Glas® 2203-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Excellent stiffness to weight rat..
Specific Gravity 1.70 - 1.85 g/cc
1.70 - 1.85 g/cc
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Specific Gravity 1.70 - 1.85 g/cc
1.70 - 1.85 g/cc
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Specific Gravity 1.70 - 1.80 g/cc
1.70 - 1.80 g/cc
ISO 1183
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Custom Resins Vexel™ E20GF45 , 45% Glass Reinforced PET  (discontinued **)
Description: Vexel™ E20GF45 is a 45% glass fiber reinforced, general purpose PET. Information provided by Custom Resins.
Specific Gravity 1.70 - 1.90 g/cc
1.70 - 1.90 g/cc
ASTM D792
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Specific Gravity 1.70 g/cc
1.70 g/cc
ISO 1183
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and ..
Specific Gravity 1.70 g/cc
1.70 g/cc
ISO 1183
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral
PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS.
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Samsung Cheil Industries Infino® XK-2307 PPS
Information provided by Samsung Cheil Industries.
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66
LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead.
Specific Gravity 1.70 g/cc
1.70 g/cc
Cured
Tra-Con Tra-Bond 546S04 Thixotropic UV/Blue Light Cure Adhesive
TRA-BOND 546S04 is a thixotropic UV/blue light curable adhesive with a secondary heat cure. TRA-BOND 546S04 is ideal for general optics bonding, mounting of lenses, and glob top applications. The ..
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Specific Gravity 1.70 - 1.86 g/cc
1.70 - 1.86 g/cc
ASTM D792
Daikin NEOFLON EP-521 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Specific Gravity 1.70 - 1.90 g/cc
1.70 - 1.90 g/cc
IEC 1212-2 8.1
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet
Specific Gravity 1.70 - 1.90 g/cc
1.70 - 1.90 g/cc
IEC 1212-2 7.2
Hippe MF GC 21 Woven Glass Cloth Reinforced Melamine Resin - Round, Rolled Tube
Used in mechanical and electrical applications. High mechanical strength. Good arc and tracking resistance. Information provided by Hippe.
Specific Gravity 1.70 g/cc
1.70 g/cc
ETFE film property; ASTM D792
Arlon 25188T017 Silicone Rubber/Laminated ETFE Film
Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion
Specific Gravity 1.70 g/cc
1.70 g/cc
silicone property; Arlon SQA-TMS-024
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Specific Gravity 1.70 g/cc
1.70 g/cc
Aremco AREMCOLOX™ 502-1600 (99%) Machinable Boron Nitride 99%
Hot-pressed high purity 99% boron nitride. High thermal conductivity. Easily machined. Non-reactive in molten salts, aluminum and other metals. Plates from 1/4" to 1" thick; rods from 1/4" to 3"..
Specific Gravity 1.70 g/cc
1.70 g/cc
Method A; ASTM D792
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..