Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® GR-5030FX SAN, Glass Filled

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded, Glass Reinforced
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® GR-5030FX SAN, Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0020 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 5.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 113 MPa
16400 psi
5 mm/min; ASTM D638
Flexural Strength 137 MPa
19900 psi
2.8 mm/min; ASTM D790
Flexural Modulus 8.83 GPa
1280 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.392 J/cm

@Thickness 3.17 mm
0.735 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 109 °C

@Thickness 6.40 mm
228 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 - 3.00 mm
HB

@Thickness 0.0591 - 0.118 in
Copyright © lookpolymers.com All Rights Reserved