Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.83 GPa | 1280 ksi | DIN 53452; ASTM D790 |
Kolon SPESIN® KP2122G30VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | DIN 53452; ASTM D790 |
Kolon KOPET® KP133135 FR-PET Resin
(discontinued **) KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of p.. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | 20% Glass RTM Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36P PC LNP* Lubricomp* DFL36P is a compound based on Polycarbonate containing 30% Glass Fiber 15% PTFE. Added features include: Exceptional Processing. Internally Lubricated. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
LG Chemical LUCON PO-5300H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Flexural Modulus | 8.83 GPa @Thickness 3.20 mm |
1280 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Flexural Modulus | 8.83 GPa @Thickness 6.40 mm |
1280 ksi @Thickness 0.252 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 8.83 GPa @Thickness 3.20 mm |
1280 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | DIN 53452; ASTM D790 |
Kolon SPESIN® KP212G30VO G/F Reinforced & Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Flexural Modulus | 8.83 GPa @Thickness 3.20 mm |
1280 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose Feature: Injection Molding, SAN+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
Gromax PBT 4130-201D 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | 5 mm/min; ISO 178 |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.83 GPa @Thickness 3.20 mm |
1280 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific) LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-5030FX SAN, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GR-5030FX SAN, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
Samyang Tripet® 2500G30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
Samyang Tripet® 2550GN30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D201G30 PBT, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | 20% Glass RTM Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60G6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60G7F Nylon 66, 35% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12 LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas .. |
|||
Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |